Reduction of Cross Contamination by Welding Process for M.S. and S.S
- Kshitij Jani
- Prof. Ashish Desai
MIG welding, TIG welding, Hardness testing, Chemical testing
Cross Contamination Defect is Occurred in Generally Metal Joining Process. In this Process Cross Contamination is Occred in Joining of Mild Steel and Stainless Steel. This Defect is occurred by Mixing of mild steel and stainless steel by arc welding process.Stainless steel is used to made of Pressure vessels,but stainless steel is high cost material,so for reducing of cost by metal joining process of ms and ss is necessary.but when metal joining process is directly done the cross contamination is occurred.For reducing this defect slots are making on ms plate and ss plates and then ss 316L is poured on it and then arc welding is done on it. To using this process in metal joining process cross contamination defect is reduced and this metal joining process mixture of SS316L and MS IS2062 is ready to made of pressure vessels.for checking of chemical composition of both metals testing procedures are required.
Kshitij Jani, Prof. Ashish Desai. "Reduction of Cross Contamination by Welding Process for M.S. and S.S".INTERNATIONAL JOURNAL OF ENGINEERING DEVELOPMENT AND RESEARCH ISSN:2321-9939, Vol.4, Issue 2, pp.534-537, URL :https://rjwave.org/ijedr/papers/IJEDR1602095.pdf
Volume 4 Issue 2
Pages. 534-537